TECAFORM® AD HPV13 brown
TECAFORM® HPV13 is a brown homopolymer acetal with an internal PTFE lubricant. Its low coefficient of friction, excellent PV values, toughness, wear resistance, and machinability make it an exceptional material for use in many industrial and military components with moving parts. Additionally, TECAFORM® HPV13 has superior chemical resistance and flexural fatigue properties, as well as low moisture absorption associated with acetal materials
Facts
Chemical Designation
POM-H (Polyacetal (Homopolymer))
Color
brown
Density
1.5 g/cm3
Fillers
PTFE powder
POM-H (Polyacetal (Homopolymer))
Color
brown
Density
1.5 g/cm3
Fillers
PTFE powder
Features
- very good slide and wear properties
- good mechanical properties
- good machinability
- good chemical resistance
- low water absorption
- good dimensional stability
Industries
food processing
food technology
conveyor technology
power engineering
gear manufacturing
packaging and paper machinery
business machines
food technology
conveyor technology
power engineering
gear manufacturing
packaging and paper machinery
business machines
Downloads
Show/Hide Mechanical Properties
Description | value | unit | condition | test method |
Modulus of elasticity (tensile test) | 380,000 | psi | @ 73 °F | ASTM D 638 |
Tensile strength at yield | 7700 | psi | @ 73 °F | ASTM D 638 |
Elongation at break (tensile test) | 10 | % | @ 73 °F | ASTM D 638 |
Flexural strength | 13,000 | psi | @ 73 °F | ASTM D 790 |
Modulus of elasticity (flexural test) | 450,000 | psi | @ 73 °F | ASTM D 790 |
Compression strength | 13,000 | psi | @ 73 °F, 10% strain | ASTM D 695 |
Compression strength | 3000 | psi | @ 73 °F, 1% strain | ASTM D 695 |
Compression modulus | 240,000 | psi | @ 73 °F | ASTM D 695 |
Impact strength (Izod) | 1.5 | ft-lbs/in | @ 73 °F | ASTM D 256 |
Rockwell hardness | 118 | R Scale @ 73 °F |
ASTM D 785 | |
Rockwell hardness | 78 | M Scale, @ 73 °F | ASTM D 785 | |
Coefficient of friction | 0.07 | Static | ASTM D 3702 | |
Coefficient of friction | 0.12 | Dynamic, 40 pis, 50 fpm | ASTM D 3702 | |
Wear rate | 20*10-10 | in³-min/ft-lbs-hr | Againt Steel, 40 psi, 50 fpm | ASTM D 3702 |
Show/Hide Thermal Properties
Description | value | unit | condition | test method |
Melting temperature | 347 | °F | ||
Deflection temperature | 244 | °F | @ 264 psi | ASTM D 648 |
Deflection temperature | 334 | °F | @ 66 psi | ASTM D 648 |
Service temperature | 185 | °F | Long Term | |
Thermal expansion (CLTE) | 6.8*10-5 | in/in/°F | range 85F to 140F | ASTM D 696 |
Show/Hide Other Properties
Description | value | unit | condition | test method |
Limiting PV | 1,600 | ft-lbs/min | @ 100 fpm | |
Limiting PV | 12,000 | ft-lbs/min | @ 10 fpm | |
Moisture absorption | 0.12 | % | @ 24 hrs, 73 °F | ASTM D 570 |
Flammability (UL94) | 6.33 mm |
Other POM-H Products: