DELRIN® Series Black (TECAFORM AD)
Delrin® 150 black is a homopolymer acetal material that is manufactured by Ensinger (using black Delrin USA LLC resin) and sold under the tradename TECAFORM AD black. Delrin 150 black exhibits a high melting point and high strength, but is sensitive to hydrolysis with continuous exposure to hot water over 140°F and steam. Black Delrin, like all other POM-H materials, holds a slightly higher density, hardness and strength than acetal POM-C. Furthermore, POM-H black has excellent wear resistance and good sliding properties, as well as an outstanding machining ability, thus, making POM-H black an extremely adaptable engineering material. Delrin is a registered trade mark of Delrin USA LLC.
Facts
Chemical Designation
POM-H (Polyacetal (Homopolymer))
Color
black
Alternative colors available:
white
Density
1.42 g/cm3
POM-H (Polyacetal (Homopolymer))
Color
black
Alternative colors available:
white
Density
1.42 g/cm3
Features
- good machinability
- high stiffness
- high fatigue strength
- high creep resistance
- good wear properties
- very good abrasion resistance
Industries
automotive industry
construction industry
conveyor technology
mechanical engineering
electronics
fixture construction
home appliances
gear manufacturing
construction industry
conveyor technology
mechanical engineering
electronics
fixture construction
home appliances
gear manufacturing
Downloads
Show/Hide Mechanical Properties
Description | value | unit | condition | test method |
Modulus of elasticity (tensile test) | 350,000 | psi | @ 73 °F | ASTM D 638 |
Tensile strength at yield | 11,000 | psi | ASTM D 638 | |
Elongation at break (tensile test) | 40 | % | @ 73 °F | ASTM D 638 |
Flexural strength | 14,000 | psi | @ 73 °F | ASTM D 790 |
Modulus of elasticity (flexural test) | 460,000 | psi | @ 73 °F | ASTM D 790 |
Compression strength | 2,700 | psi | @ 73 °F, 1% strain | ASTM D 695 |
Compression strength | 14,000 | psi | @ 73 °F, 10% strain | ASTM D 695 |
Compression modulus | 460,000 | psi | @ 73 °F | ASTM D 695 |
Impact strength (Izod) | 1.5 | ft-lbs/in | @ 73 °F | ASTM D 256 |
Rockwell hardness | 120 | @ 73 °F R Scale |
ASTM D 785 | |
Coefficient of friction | .2 | Dynamic 40 psi, 50 fpm |
ASTM D 3702 | |
Wear rate | 55*10-10 | in³-min/ft-lbs-hr | 40 psi, 50 fpm | ASTM D 3702 |
Show/Hide Thermal Properties
Description | value | unit | condition | test method |
Melting temperature | 347 | °F | ASTM D 2133 | |
Deflection temperature | 208 | °F | @1.80 MPa | ISO-R 75 Method A |
Service temperature | 300 | °F | Intermittent | |
Service temperature | 185 | °F | Long Term |
Show/Hide Other Properties
Description | value | unit | condition | test method |
Moisture absorption | .90 | % | @ saturation, 73 °F | ASTM D 570 |
Other POM-H Products: