TECARAN ABS natural
Ensinger TECARAN ABS material is a terpolymer and an amorphous resin. It is manufactured by combining three different compounds. The three that make up TECARAN ABS are acrylonitrile, butadiene, and styrene. TECARAN ABS occupies the unique position of being a bridge between the general industrial and other higher performance engineering thermoplastics. Its performance is characterized by toughness and impact strength even at low temperatures, good stiffness and machinability.
Facts
Chemical Designation
ABS (Acrylnitrile-butadiene-styrene copolymer)
Color
beige opaque
Alternative colors available:
black
Density
1.02 g/cm3
ABS (Acrylnitrile-butadiene-styrene copolymer)
Color
beige opaque
Alternative colors available:
black
Density
1.02 g/cm3
Features
- electrically insulating
- high stiffness
- good chemical resistance
- low density
- good damping
- high toughness
- low moisture absorption
Industries
food processing
home appliances
automotive industry
fixture construction
food engineering
electronics
medical technology
home appliances
automotive industry
fixture construction
food engineering
electronics
medical technology
Downloads
Show/Hide Mechanical Properties
Description | value | unit | condition |
test method |
modulus of elasticity (tensile test) | 400,000 | psi | @ 73 °F | ASTM D 638 |
Tensile strength at yield | 5,800 | psi | @ 73 °F | ASTM D 638 |
Tensile strength at break | 4,000 | psi | @ 73 °F | ASTM D 638 |
Elongation at yield (tensile test) | 2.0 | % | @ 73 °F | ASTM D 638 |
Elongation at break (tensile test) | 30 | % | @ 73 °F | ASTM D 638 |
Flexural strength | 8,900 | psi | @ 73 °F | ASTM D 790 |
Modulus of elasticity (flexural test) |
310,000 | psi | @ 73 °F | ASTM D 790 |
Compression strength | 3,200 | psi | @ 73 °F, 1% strain | ASTM D 695 |
Compression strength | 7,100 | psi | @ 73 °F, 10% strain | ASTM D 695 |
Compression modulus | 375,000 | psi | @ 73 °F | ASTM D 695 |
Impact strength (Izod) | 5.3 | ft-lbs/in | @ 73 °F | ASTM D 256 |
Rockwell hardness | 108 | @ 73 °F | ASTM D 785 | |
Shore hardness | 78 | @ 73 °F | ASTM D 2240 | |
Coefficient of friction | 0.19 - 0.21 | Static | ASTM D 3702 | |
Coefficient of friction | 0.35 | Dynamic, 40 psi, 50 fpm | ASTM D 3702 | |
Wear (K) factor | 3500*10-10 | in³-min/ft-lbs-hr | Against Steel, 40 psi, 50 fpm | ASTM D 3702 |
Show/Hide Thermal Properties
Description | value | unit | condition |
test method |
Vicat softening point | 224 | °F | ||
Glass transition temperature | 220 | °F | ASTM D 3418 | |
Deflection temperature | 200 | °F | @ 66 psi | ASTM D 648 |
Deflection temperature | 177 | °F | @264 psi | ASTM D 648 |
Service temperature | 210 | °F | Intermittent | |
Service temperature | 160 | °F | Long Term | |
Thermal expansion (CLTE) | 5.6*10-5 | in/in/°F | -40F to 100F | ASTM D 696 |
Show/Hide Electrical Properties
Description | value | unit | condition |
test method |
surface resistivity | 1.0*1014 | Ω/square | ASTM D 257 | |
volume resistance | 1*1015 | Ω*cm | ASTM D 257 | |
Dielectric strength | 450 | V/mil | ASTM D 149 | |
Dissipation factor | 0.02 | @ 60 Hz, 73 °F | ASTM D 150 | |
Dielectric constant | 3.3 | @ 60 Hz, 73 °F, 50% RH | ASTM D 150 |
Show/Hide Other Properties
Description | value | unit | condition |
test method |
Moisture absorption | 0.13 | % | @ 24 hrs, 73 °F | ASTM D 570 |
Moisture absorption | 0.70 | % | @ saturation, 73 °F | ASTM D 570 |
Flammability (UL94) | HB |